時間: 人気:0タイムズ
適用基準:
主なパラメータ (Table 1):
パラメータ | Range/Specification |
---|---|
Temperature Control | 100–200°C (±0.3°C stability) |
Oscillation Frequency | 1.7 Hz (standard), 0.5–2 Hz adjustable |
Strain Amplitude | ±0.5° angular or ±0.05 mm linear |
Torque Measurement | 0–20 N·m (resolution: 0.001 N·m) |
Sample Volume | 3–5 cm³ (cylindrical mold) |
Data Output | Real-time torque-time curves |
動作原理:
The tester operates by sealing a rubber specimen in a two-part mold cavity. One section oscillates with a small-amplitude motion (angular or linear), inducing shear strain, while the other remains stationary. A transducer measures the torque response, which correlates with the material’s viscoelastic changes during curing. Key metrics derived include:
しけんげんり:
The test simulates industrial curing conditions by heating the specimen to a predefined temperature. As crosslinking begins, the torque increases due to rising shear modulus. The instrument plots torque vs. time curves, enabling calculation of cure rates and activation energy. Advanced models incorporate temperature compensation algorithms to minimize thermal gradients, ensuring repeatability. By comparing torque increments (e.g., 90% of MH), manufacturers optimize formulations for specific applications, such as high-rebound soles or oil-resistant seals.
適用#テキヨウ#:
This equipment’s precision and compliance with international standards make it indispensable for modern rubber labs, ensuring products meet durability and safety requirements.