適用基準

The tester adheres to international standards for material testing at low temperatures, including:

  • ISO 4674-2 (Rubber- or plastics-coated fabrics – Determination of low-temperature bend test)
  • ASTM D1790 (Standard test method for resistance of organic coatings to the effects of rapid deformation (impact))
  • GB/T 2423 (China’s national standard for environmental testing – Cold tests)
  • EN 60068-2-1 (Environmental testing – Cold tests for electronic components)
  • SAE J2339 (Cold temperature impact resistance for automotive coatings)

These standards ensure consistent evaluation of material behavior under thermal and mechanical stress.

主なパラメータ


パラメータ仕様
おんどはんい-70°C to +200°C (adjustable via cryogenic cooling)
Bending Angle0–180° (adjustable for different material flex requirements)
Stroke Frequency50–300 cycles/min (programmable)
Sample Dimensions100 × 20 mm (standard for coatings/films); up to 300 × 50 mm (customizable)
Cooling SystemLiquid nitrogen or mechanical refrigeration (LC-120 model)
Control SystemPLC-based with 7-inch touchscreen (multilingual interface)
電源装置220V/50Hz, 800W
寸法すんぽう800 × 600 × 1500 mm (L × W × H)

動作原理

The tester operates by combined thermal and mechanical stress:

  1. Temperature Conditioning: Samples are cooled to -70°C in a climate chamber.
  2. Bending Cycle: A motorized arm repeatedly bends the sample at a preset angle (e.g., 90° or 180°) and frequency (e.g., 100 cycles/min).
  3. Cycle Execution: The test runs until surface cracks appear, or a predefined cycle count (e.g., 20,000 cycles) is reached.
  4. Damage Assessment: Post-test, samples are evaluated for cracking, delamination, or coating failure using microscopy or visual grading.

Test Principle & Applications

  • Cold Flexibility Testing (ISO 4674-2/ASTM D1790):
    • Samples are bent 10,000–50,000 times at -40°C to simulate polar or alpine conditions.
    • Results are graded based on crack appearance:
      • Pass: No visible cracks or coating separation.
      • Fail: Cracks exceeding 0.5 mm in width.
  • Key Industries:
    • 航空宇宙: Validating aircraft fuel lines and sealants.
    • じどうしゃ: Testing battery packs and exterior trim for electric vehicles.
    • Construction: Assessing pipe insulation and roofing membranes.

The Low-Temperature Bending Resistance Tester is indispensable for manufacturers developing products for extreme climates, ensuring reliability and compliance with regulatory standards. Its precision and adaptability make it a cornerstone of materials testing in harsh environments.

免責事項: 上記のコンテンツは,業界内部者のみの参照およびコミュニケーションのためであり,その正確性または完全性を保証しません.関連法規および本ウェブサイトの規制により,関連品を購入するユニットまたは個人は,有効な資格および資格条件を取得する必要があります.


オンラインメッセージ

連絡先情報

会社電話

+86-21-6420 0566

営業時間

月曜日から金曜日

携帯電話:

13816217984

メール:

info@qinsun-lab.com

QRコード